Verfahren zur Herstellung eines Hochsicherheitskohlenstoffmaterials

EP4768433 1. Juli 2026

Anmelder: CPC Corporation, Taiwan 🇹🇼

Details

Veröffentlichungs-Nr.
EP4768433
Anmeldetag
28. Februar 2025
Veröffentlichung
1. Juli 2026
Rechtsraum
EP
Offizieller Volltext

Abstract

A method for manufacturing a high-safety carbon material includes: step (A), mixing a carbon material, a coating material, glutaraldehyde and a solution with a weight ratio of 100:2-6:0.2-0.6:100-300 to form a mixed slurry, wherein the carbon material is soft carbon and/or artificial graphite, and the coating material is chitosan and/or sulfonated chitosan; step (B), stirring the mixed slurry evenly and heating at 70°C-90°C to form an evaporated slurry; step (C), heating the evaporated slurry at 70°C-90°C for 24 hours or more, and then cooling to room temperature to form a high-safety carbon material. The method is helpful to obtain a high-safety carbon material, which can slow down a large amount of heat release when a solid-state electrolyte interface decomposes, prevent the heat generated by the decomposition of the solid-state electrolyte interface from triggering the overall thermal runaway mechanism, and can improve the safety of anode materials used in batteries.

Anmelder

Firma
CPC Corporation, Taiwan
Land
🇹🇼 Taiwan

Noch Fragen?

Wir helfen Ihnen gerne weiter. Schreiben Sie uns einfach.

Kontakt aufnehmen