Verfahren zur Herstellung eines Mineralschaums aus einem Schäumenden Schlamm mit Hoher Streckgrenze

EP4768458 1. Juli 2026

Anmelder: Holcim Technology Ltd. 🇨🇭

Details

Veröffentlichungs-Nr.
EP4768458
Anmeldetag
24. Dezember 2024
Veröffentlichung
1. Juli 2026
Rechtsraum
EP
Offizieller Volltext

Abstract

The invention relates to a method for the production of a mineral foam comprising the following steps: (i) preparing a cement slurry, comprising: - a cementitious composition; - a carboxylic acid or salt thereof selected from the group consisting of a monocarboxylic acid comprising from 1 to 5 carbon atoms, a dicarboxylic acid comprising from 2 to 5 carbon atoms and mixtures thereof; and - water; wherein the carboxylic acid or salt thereof is present in an amount from 0.6% to 2.5%, preferably from 0.6% to 2%, in weight relative to the total dry weight of the cementitious composition, (ii) adding to the cement slurry obtained after step (i) a gas-forming liquid comprising a gas-forming agent to obtain a foaming slurry; (iii) applying the foaming slurry obtained in step (ii) on a support.

Anmelder

Firma
Holcim Technology Ltd.
Land
🇨🇭 Schweiz
🇨🇭 Holcim Technology

Holcim Technology ist die Schweizer Technologiegesellschaft des Baustoffkonzerns Holcim mit Sitz in Zug, zuständig für Forschung im Bereich Zement und Baustoffe. Das Patentportfolio konzentriert sich stark auf anorganische Chemie und Werkstoffe, ergänzt durch Fertigungs- und Gebäudetechnik. Anmeldungen laufen durchgehend seit 2003.

364 Patente in unserer Datenbank

Vertreten von

Noch Fragen?

Wir helfen Ihnen gerne weiter. Schreiben Sie uns einfach.

Kontakt aufnehmen