Verfahren zur Wiederherstellung von Legierungsverarmung in einer Schaufel um Kühlbohrungen
Anmelder: RTX Corporation 🇺🇸
Details
- Veröffentlichungs-Nr.
- EP4786731
- Anmeldetag
- 16. Januar 2026
- Veröffentlichung
- 5. August 2026
- Rechtsraum
- EP
Abstract
A method of reducing depletion of elements from an airfoil (140) includes disposing a bond coating on the airfoil (140), where the airfoil (140) comprises cooling channels (150). The airfoil (140) includes a material that has an initial composition. A cooling hole (150a) is machined in the airfoil (140) to contact the cooling channels (150) such that a fluid travelling in the cooling channel (150) may be discharged via the cooling hole (150a). The machining of the cooling hole (150a) results in a formation of a depleted region around the cooling hole (150a). The depleted region is depleted of a portion of the initial composition of the airfoil (150). A top coat is disposed on the bond coat. The airfoil (150) is subjected to a heat treatment at a temperature effective to promote diffusion of elements from a non-depleted region to the depleted region around the cooling hole.
Anmelder
- Firma
- RTX Corporation
- Land
- 🇺🇸 USA
US-amerikanischer Luft- und Raumfahrt- sowie Verteidigungskonzern, entstanden aus Raytheon und United Technologies. Entwickelt und fertigt Triebwerke, Avionik, Radarsysteme, Raketen- und Verteidigungstechnik für zivile und militärische Kunden.
10.502 Patente in unserer Datenbank